Hubei Nuojin Sen Technology Co.,Ltd

Self-improvement, practical effectiveness

Manufacturer from China
Active Member
7 Years
Home / Products / Photoimageable Solder Mask /

Green Color PCB Printing Curable Photoimageable Solder Mask Ink Fineness ≤8µM

Contact Now
Hubei Nuojin Sen Technology Co.,Ltd
City:wuhan
Province/State:hubei
Country/Region:china
Contact Now

Green Color PCB Printing Curable Photoimageable Solder Mask Ink Fineness ≤8µM

Ask Latest Price
Video Channel
Brand Name :NUOJINSEN
Model Number :101
Certification :ROHS,SGS
Place of Origin :China
MOQ :100kgs
Price :Negotiation
Payment Terms :T/T,LC
Supply Ability :100000kgs/month
Delivery Time :7-10days
Packaging Details :1kg,5kg,10kg,20kg
Color :Black
Fineness :≤8µm
Mix ratio :Base/Hardener=3:1
Solid content after mixing :75±3%
Viscosity after mixing (25℃) :200±30 dPa﹒s
Density after mixing (25℃) :1.30 ~1.50 g/ml
Pot life after mixing :24 hour
Environment standard :In compliance with RoHS directives
Halogen content :≤600ppm
Pre-baking :75℃ , 70 min
Exposure energy :300 ~600 mJ/cm2
Shelf life :6 months since the date of manufacture
more
Contact Now

Add to Cart

Find Similar Videos
View Product Description

Black color pcb ink,photoimageable curable solder resist mask

Items Features Notes
Color Green
Fineness ≤8µm 0 ~25µm Fineness gauge
Mix ratio Base/Hardener=3:1 Weight ratio
Solid content after mixing 75±3% Surface printing ink
82±3% tamponade series
Viscosity after mixing (25℃) 200±30 dPa﹒s VT-04FSurface printing ink
300±50 dPa﹒s VT-04F tamponade series
Density after mixing (25℃) 1.30 ~1.50 g/ml
Pot life after mixing 24 hour Store below 25℃ in dark
Environment standard In compliance with RoHS directives SGS testing
Halogen content ≤600ppm Only KSM-S6188 E series
Pre-baking limit 75℃ , 70 min
Exposure energy 300 ~600 mJ/cm2 The effective value through the polyester film
Package Base :750g , Hardener :250 g According to customer requirements
Base :3kg , Hardener :1kg
Shelf life 6 months since the date of manufacture Store 10~25℃ in dark

Working procedure

1. Mixing

Mixing a small amount main agent with hardener and stirring thoroughly,then mixing the mixture above with the remanent main agent,add appropriate diluent and stirring 5-10 minutes. The viscosity of ink is adjusted to 120 PS if printed by hand. And it is adjusted to 180 PS if printed by machine.It is adjusted to 200 PS if it is aluminum tamponade .The viscosity of ink mixed above is measured at 25 degrees. Please use the special diluent of our company if the viscosity of ink needs to adjust.

  • Remain time

10-15 minutes after stiring uniformly

  • Ordinary boards:43T;Chemical-plating Aurum or Tin boards:36T
  • Pre-baking

1) Single side printing separately

First side:72-76 degrees,15-18 min

Second side:72-76 degrees,30-35 min

  • Double sides printing simultaneously:72-76 degrees,40-60min
  • Exposure

300-500mJ/cm2,Black ink:600-750mJ/cm2,exposure step:10-12 steps

  • Developing:

Developing solution:0.8-1.2wt% Na2CO3 or K2CO3 aqueous solution

Developing solution temperature:28-32 degrees

Spray pressure:1.5-2.5kg/cm2

Developing time:40-90 seconds

  • Post cure

Spray Tin board:150 degrees*(60-120min)

Chemical-plating Aurum board:150 degrees*(50-60min)

Thick copper plate,boards printed with black ink should be post-black in subsection:75 degrees*(60-120min)+100 degrees*30 min+150 degrees*(60-90min)

  • Safe time

6 months since the date of manufacture,store below 25 degree in dark

  • Attention:

1) Mixing the ink fully before using

2) We will offer you special diluent or PMA if the ink need dilute

3) The values above are based on experiments in our lab.Experiments need to be carried out in order to get proper using condition.

Inquiry Cart 0